(KTiOAsO4)
KTA
(potassium titanyl arsenate)
Compound |
KTiOAsO4 |
|
Transparency range, µm |
0.35 – 5.5 |
|
Nonlinear coefficient, pm/V |
d31= 2.76; d32= 4.74; d33= 18.5 |
|
Symmetry |
Orthorhombic, mm2 point group |
|
Cell parameters, Å |
a=13.103, b=6.558, c=10.746 |
|
Typical Reflection indices |
1064 nm 532 nm |
nx=1.7826, ny=1.7890, nz=1.8677 nx=1.8293, ny=1.8356, nz=1.9309 |
Optical Damage Threshold, GW/cm2 |
1064 nm
(t=10 ns) |
1.5 |
Electrooptic coefficients, pm/V |
r13=15, r23=21, r33=40 | |
Mohs hardness |
5 |
The parameters of optical elements
Orientation accuracy, arc min< 30<td20/10
Parallelism, arc sec | < 30 | |
Flatness | 546 nm | λ/6 |
Surface quality, scratch/dig |
Application
- Optical parametric oscillator (OPO) in middle IR region 1 – 5.5 µm
- Different frequency generation in middle IR region 1 – 5.5 µm
We are able to provide suitable Anti-reflection / Protective, etc. coatings tailored to customer’s specifications, reflectivity curves are applied upon request.